Development Process
40+ quality checkpoints from raw steel to finished blade.
Material Receiving
Certified steel billets spectrographically analyzed for chemical composition.
Forging & Annealing
Steel heated to 1050°C, precision-forged, then slowly cooled to relieve internal stresses.
Cryogenic Hardening
Blades deep-frozen to -70°C, transforming retained austenite to martensite.
Grinding & Assembly
CNC precision grinding to final geometry. Hand-assembled with handle scales.